Solving D2 Chipping Issues: Why DC53 High-Toughness Cold Work Steel Doubles Die Life in Punching Inserts
The press stops in the middle of the production run. The operator has started seeing burrs on the parts. A few pieces are pulled from

The press stops in the middle of the production run. The operator has started seeing burrs on the parts. A few pieces are pulled from

The press is running at full speed when the first bad parts appear. The operator notices a small burr on the stamped edge. Then another.

The press has stopped. Again. The operator has found fresh burrs on the stamped parts. Someone pulls the parts from the last few cycles and

The stamping line is running at full speed. Then the operator starts noticing burrs on the parts. The die was working fine yesterday. It has

“Can we use Cr12MoV instead of D2?” This is a pretty normal question when we quote steel for a large stamping die. And honestly, sometimes

The problem usually gets noticed after heat treatment. A heavy stamping die goes into the furnace looking right. When it comes out, a few dimensions

The mold is still producing parts, but the cavity surface is starting to show small pits. With PVC or other chemically aggressive plastics, this is

If you are choosing stainless steel for a medical mold insert, precision tooling component, or wear part, the question is usually not simply “Is 440C

The Mold Was Already Using S136. So Why Change It? A medical mold manufacturer came to us with a problem that was not unusual. They

The Problem Usually Starts During Polishing A customer making transparent medical components came to us with a familiar problem. The cavity had to reach SPI